Common problems and solutions for the use of PVC plastic film

In the process of shrinking packaging of PVC plastic film, some problems such as flatulence, atomization and fish eye of plastic film are often encountered.
These problems can be corrected by adjusting machine settings. The most frequently adjusted packaging machine's temperature, circulation air velocity, conveyor speed, number of air holes and plastic film size.
PVC plastic envelope packaging use problem 1:
• flatulence
Hot air is retained in plastic film
Solution:
1. Increase the number of air permeable holes to expedite the leakage of air from the plastic film
2, slow down the speed of the conveyor belt, so that the hot air is leaking from the plastic film for a long time.
3. The temperature of the high packing machine helps to leak out the air from the plastic film
PVC plastic envelope packaging use problem two:
• atomization
The surface of the plastic film became blurred, like a mist
Solution:
1. Reducing the temperature of the packing machine and the high temperature are the causes of the atomization of plastic film.
2, adjust the speed of the conveyer belt of the packing machine, and reduce the time of the plastic sealing film to contact the heat.
PVC plastic envelope packaging use problem three:
Fish eye
A fish eye shaped wrinkle on the surface of a plastic film
Solution:
1. The temperature of the shrink packing machine is too low to raise the temperature of the packing machine.
2. The speed of the conveyor belt is too fast to reduce the speed of the conveyor belt.
3. The circulation wind of the shrink packing machine is too low to turn the circulating wind down